Mechanical Properties Metric English Comments
Peel Strength 10.0 - 12.0 kN/m
57.1 - 68.5 pli
Cured for 15 mins at 200°C
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Peel Strength >= 10.0 kN/m
>= 57.1 pli
3-layer at 80°C; DIN 30678
Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating
Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108..