Mechanical Properties Metric English Comments
Peel Strength 1.38487 - 1.84065 kN/m

@Temperature 288 - 288 °C
7.90207 - 10.5027 pli

@Temperature 550 - 550 °F
Average value: 1.67 kN/m Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Peel Strength 1.38487 - 1.84065 kN/m

@Time 10.0 - 20.0 sec
7.90207 - 10.5027 pli

@Time 0.00278 - 0.00556 hour
Average value: 1.67 kN/m Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..