Peel Strength 2.04 - 3.40 kN/m
11.6 - 19.4 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-330 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo..