Polymer Property : Peel Strength = 13.3 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9320 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9410 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Peel Strength 2.33 kN/m
13.3 pli
After 2 week exposure to 71°C, Vinyl-Altro to Composite, 2 surface Bond
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive
Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor..
Peel Strength 2.33 kN/m
13.3 pli
(S1 to S1), Bond Strength; Arlon SQA-TMS-011
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Peel Strength 2.33 kN/m

@Temperature 23.0 °C
13.3 pli

@Temperature 73.4 °F
Aluminum, etched, Bell Peel, Adhesive Failure; ASTM D3167
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..