Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.68 kN/m | 15.3 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |