Polymer Property : Peel Strength = 160 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 28.0 kN/m
160 pli
Impact Peel
Dow BETAMATE™ 1496 V Epoxy
BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle..