Polymer Property : Peel Strength = 2.19 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.19 kN/m
12.5 pli
Adhesion to Steel; ASTM D1000
3M Scotch™ 2200 Vinyl Mastic Pads and Rolls
3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d..
Peel Strength 2.19 kN/m
12.5 pli
Adhesion to Polyethylene; ASTM D1000
3M Scotch™ 2200 Vinyl Mastic Pads and Rolls
3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d..
Peel Strength 2.19 kN/m
12.5 pli
Adhesion to Steel; ASTM D1000
3M Scotch™ 2210 Vinyl Mastic Pads and Rolls
3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d..
Peel Strength 2.19 kN/m
12.5 pli
Adhesion to Polyethylene; ASTM D1000
3M Scotch™ 2210 Vinyl Mastic Pads and Rolls
3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d..
Peel Strength 2.19 kN/m
12.5 pli
Bond Strength; ASTM D624
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe..
Peel Strength 2.19 kN/m
12.5 pli
(S1 to S1), Bond Strength; Arlon SQA-TMS-011
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..