Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.23 kN/m | 12.7 pli | Copper; 1/2 oz. EDC After Solder Float; IPC-TM-650 2.4.8 |
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Peel Strength | 2.23 kN/m | 12.7 pli | (S2 to S2), Bond Strength; Arlon SQA-TMS-011 |
Arlon 51808R011 0.011" (0.279 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat This data represents typical values for the production .. |