Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.72 - 4.08 kN/m | 15.5 - 23.3 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-731 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Peel Strength | 2.72 - 4.08 kN/m | 15.5 - 23.3 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-733 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Peel Strength | 2.72 - 4.08 kN/m | 15.5 - 23.3 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-737 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Peel Strength | 2.72 kN/m | 15.5 pli | Wood -Supported Vinyl, 180°, Aging 1 Day @ RT |
3M Scotch-Weld™ 2262 Plastic Adhesive Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very .. |