Mechanical Properties Metric English Comments
Peel Strength 2.75 kN/m
15.7 pli
Valley Adhesives EM-220 Low Temperature Application Glue Stick
Valley Adhesives EM-220 Low Temperature Application Glue StickBonds many plastics, polyolefins and light weight heat sensitive materials.
Peel Strength 2.75 kN/m
15.7 pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Treated plywood, 2 surface Bond
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive
Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor..