Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.49303 kN/m | 2.8125 pli | Initial, Linered side-PVC; ASTM D3330 |
3M 2205 Thin Flexographic Plate Mounting Tape 3M™ Thin Flexographic Mounting Tape 2205 is a double coated film tape constructed of a polyester film carrier with differential adhesives specifically designed for the corrugated printing business .. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Non-Linered Initial, Stainless Steel; ASTM D3330 |
3M 2205 Thin Flexographic Plate Mounting Tape 3M™ Thin Flexographic Mounting Tape 2205 is a double coated film tape constructed of a polyester film carrier with differential adhesives specifically designed for the corrugated printing business .. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Steel; ASTM D3330 |
3M 2E98P/S2K Polyethylene Protective Tape 3M™ Protective Tape is a self-wound clear and printed tapes made from a co-extruded multi-polymer backing coated with a very high-tack acrylic adhesive system to help provide temporary protection o.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330 |
3M 9425 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Steel; ASTM D3330 |
3M 9497 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | to Steel; ASTM D3330 |
3M 9499 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | to Stainless Steel, 20 min dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330 |
3M 965 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1915S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 3782 Performance Continuous Taping System Tape Scotch® Performance Continuous Taping System Tapes 3782 is a packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. These tapes.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Granite; ASTM D3330 |
3M 507 Sandblast Stencil 3M™ Sandblast Stencil 507, also know as butter cut, is a general purpose sandblast stencil used for hand-cut and die-cut applications.Information provided by 3M |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7731FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Faceside; ASTM D3330 |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1915 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 353 High Performance Box Sealing Tape Scotch® Box Sealing Tape 351 is a high performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a strong abrasion resistan.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 371 Industrial Box Sealing Tape Scotch® Box Sealing Tape 371 is an industrial packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consistent pr.. |
|||
Peel Strength | 0.49303 kN/m | 2.8125 pli | Adhesion to Steel; ASTM D3330 |
3M Tartan™ 860 Strapping Tape The polypropylene backing of Tartan™ Strapping Tape 860 provides abrasion, moisture and scuff resistance. The adhesives is specifically formulated to provide good adhesion to metallic, plastic, fib.. |