Polymer Property : Peel Strength = 20.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength >= 20.0 kN/m
>= 114 pli
3-layer; DIN 30678
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating
Borcoat BB125E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the top-coat polypropylene Borcoat BB108E-1199.B..
Peel Strength >= 20.0 kN/m
>= 114 pli
3-layer; DIN 30678
Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating
Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108..
Peel Strength >= 20.0 kN/m
>= 114 pli
3-layer; DIN 30678
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating
Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c..