Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.625 - 3.50 kN/m | 14.98 - 20.0 pli | |
Permabond TA4810 Toughened Acrylic Adhesive PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac.. |
|||
Peel Strength | 2.625 - 3.50 kN/m | 14.98 - 20.0 pli | |
Permabond TA4820 Structural Acrylic Adhesive PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac.. |
|||
Peel Strength | 0.877 - 3.51 kN/m | 5.00 - 20.0 pli | Average value: 2.48 kN/m Grade Count:6 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Peel Strength | 2.63 - 3.51 kN/m | 15.0 - 20.0 pli | |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black Information provided by ITW Devcon |
|||
Peel Strength | 2.63 - 3.51 kN/m | 15.0 - 20.0 pli | |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White Information provided by ITW Devcon |