Polymer Property : Peel Strength = 200 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength >= 200 kN/m
>= 1140 pli
20+5°C; ISO 21809-1
Lushan PR298 Polypropylene Copolymer Adhesive for Steel Pipe Coating
Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&..