Mechanical Properties Metric English Comments
Peel Strength 3.30 kN/m
18.8 pli
T-Peel (CRS St 1203, 0.5mm)
Dow BETAMATE™ XW 1185 Epoxy
BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi..