Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 5.60 - 6.40 kN/m | 32.0 - 36.5 pli | Cured for 1 hr at 80°C |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |