Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.799 - 1.10 kN/m | 4.56 - 6.28 pli | Copper; 1/2 EDC foil (18 micron); Condition A; IPC-TM-650 2.4.8 |
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav.. |
|||
Peel Strength | 0.800 kN/m | 4.56 pli | Bell Peel |
Henkel Hysol EA 9323 Paste Adhesive System Viscous, but pourable, liquid adhesive that yields tough, durable adhesive bonds over a wide temperature range.Application: Structural Repair |