Polymer Property : Peel Strength = 46.2 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 8.10 kN/m
46.2 pli
Final
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl..