Mechanical Properties Metric English Comments
Peel Strength 0.8925 kN/m

@Treatment Temp. 204 °C,
Time 3600 sec
5.093 pli

@Treatment Temp. 399 °F,
Time 1.00 hour
To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.8925 kN/m

@Treatment Temp. 204 °C,
Time 3600 sec
5.093 pli

@Treatment Temp. 399 °F,
Time 1.00 hour
To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.8925 kN/m

@Treatment Temp. 204 °C,
Time 3600 sec
5.093 pli

@Treatment Temp. 399 °F,
Time 1.00 hour
To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.8925 kN/m

@Treatment Temp. 204 °C,
Time 3600 sec
5.093 pli

@Treatment Temp. 399 °F,
Time 1.00 hour
To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.8925 kN/m

@Treatment Temp. 204 °C,
Time 3600 sec
5.093 pli

@Treatment Temp. 399 °F,
Time 1.00 hour
To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket