Mechanical Properties Metric English Comments
Peel Strength 0.701 - 5.47 kN/m
4.00 - 31.2 pli
Average value: 2.39 kN/m Grade Count:11
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..