Polymer Property : Peel Strength = 6.11 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.07 kN/m
6.11 pli
to polyethylene, 180° peel test, rate of peel = 300mm/min at 25°C
Kuraray SEPTON® A1 Hot Melt Adhesive
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block c..