Polymer Property : Peel Strength = 6.375 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.118 kN/m
6.375 pli
ABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
3M 9672LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Peel Strength 1.118 kN/m
6.375 pli
Stainless Steel, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
3M ScotchCal™ 3690E Graphic Film Material
3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di..
Peel Strength 1.118 kN/m
6.375 pli
Stainless Steel, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
3M ScotchCal™ 3698E Graphic Film Material
3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di..
Peel Strength 1.118 kN/m
6.375 pli
Stainless Steel, Backside, 180° Peel, 2 mil Al
3M XR4123 Double Coated Film Tape
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o..
Peel Strength 1.118 kN/m
6.375 pli
ABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
Peel Strength 1.118 kN/m
6.375 pli
ABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
3M 9472LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..