Polymer Property : Peel Strength = 6.50 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.14 kN/m
6.50 pli
Adhesion Strength, Tape Property; Arlon SQA-TMS-047
Arlon A3015-R004-12 0.015" (0.381 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  
1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film This..
Peel Strength 1.14 kN/m
6.50 pli
To Copper (1 oz./35 micron; IPC TM-650 2.4.8
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply
Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal ..
Peel Strength 1.14 kN/m
6.50 pli
180° peel, PET/s.s.
Dielectric Polymers NT-988 High Tack Laminating Adhesive  (discontinued **)
Acrylic copolymer adhesive with silicone treated release paper liner.Features: Excellent adhesion to low surface energy substratesCompatible with most printing inksApplications: Mounting a wide vari..
Peel Strength 1.14 kN/m
6.50 pli
Bond Strength; ASTM D624
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc..