Polymer Property : Peel Strength = 6.8125 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.1942 kN/m
6.8125 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
3M 9672LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Peel Strength 1.1942 kN/m
6.8125 pli
Stainless Steel, 90° Peel, 72 hr dwell; ASTM D3330
3M 9017FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials 9017FL and 9018FL are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. T..
Peel Strength 1.1942 kN/m
6.8125 pli
Stainless Steel, 90° Peel, 72 hr dwell; ASTM D3330
3M 9018FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials 9017FL and 9018FL are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. T..
Peel Strength 1.1942 kN/m
6.8125 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
Peel Strength 1.1942 kN/m
6.8125 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
3M 9472LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..