Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.205 kN/m | 6.875 pli | PC, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330 |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 1.205 kN/m | 6.875 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330 |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 1.205 kN/m | 6.875 pli | ABS, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330 |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 1.205 kN/m | 6.875 pli | PP, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330 |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |