Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 11.7 kN/m | 67.0 pli | 180°, Polyacrylic |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |