Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 12.3 kN/m | 70.0 pli | 180°, PVC, Cotton duck failed during testing |
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 12.3 kN/m | 70.0 pli | 180°, ABS, Cotton duck failed during testing |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 12.3 kN/m | 70.0 pli | 180°, PVC, Cotton duck failed during testing |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 12.3 kN/m | 70.0 pli | 180°, ABS |
3M Scotch-Weld™ TE031 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |