Mechanical Properties Metric English Comments
Peel Strength 1.4353 kN/m
8.1875 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 2.3 mil; ASTM D3330
3M 9502 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 1.4353 kN/m
8.1875 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 2.3 mil; ASTM D3330
3M 9505 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 1.4353 kN/m
8.1875 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 2.3 mil; ASTM D3330
3M 9552 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 1.4353 kN/m
8.1875 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 2.3 mil; ASTM D3330
3M 9555 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..