Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.51 kN/m | 8.60 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi.. |
|||
Peel Strength | 1.51 kN/m | 8.60 pli | Bond Strength; Arlon-SQA-TMS-011 |
Arlon 51268R015P 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data r.. |
|||
Peel Strength | 1.51 kN/m | 8.60 pli | Bond Strength (S1 to S2); Arlon SQA-TMS-011 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |