Polymer Property : Peel Strength = 8.80 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.54 kN/m
8.80 pli
180°, Gelcoat, 50% RH
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Peel Strength 1.54 kN/m
8.80 pli
180°, Gelcoat, 50% RH
3M 4000 UV 6580 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Peel Strength 1.54 kN/m
8.80 pli
180°, Gelcoat, 50% RH
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Peel Strength 1.54 kN/m
8.80 pli
Bond Strength; ASTM D624
Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..