Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Multi-axial Impact @ -30°C Total Energy | 169 J @Thickness 25.4 mm |
125 ft-lb @Thickness 1.00 in |
ASTM D3763 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Multi-axial Impact @ -30°C Total Energy | 169 J @Thickness 25.4 mm |
125 ft-lb @Thickness 1.00 in |
ASTM D3763 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |