Mechanical Properties Metric English Comments
Flexural Toughness 0.0517 MPa
7.50 psi
ASTM D790
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic
HYTAC-FLXT is a unique material, combining the toughness and higher friction of FLX with improved release characteristic through PTFE impregnation. The result is a new, tough syntactic with just th..