Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 75.0 MPa @Temperature 23.0 °C |
10900 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 75.0 MPa @Temperature -40.0 °C |
10900 psi @Temperature -40.0 °F |
Practical Use; ASTM-D638 |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |