Polymer Property : Tensile Strength, Ultimate = 1170 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1170 MPa

@Temperature 300 °C
170000 psi

@Temperature 572 °F
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki..