Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 867 MPa

@Thickness 12.7 mm
126000 psi

@Thickness 0.500 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Ultimate 867 MPa

@Thickness 12.7 mm,
Temperature 760 °C
126000 psi

@Thickness 0.500 in,
Temperature 1400 °F
As Welded, Solution Annealed, and Aged; Base/Base Fracture
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..