Polymer Property : Tensile Strength, Ultimate = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa

@Temperature -40.0 °C
13100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.1%); ASTM-D638
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature 80.0 °C
13100 psi

@Temperature 176 °F
Practical Use (Water Absorption 2.0%); ASTM-D638
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature -40.0 °C
13100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D638
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature 23.0 °C
13100 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.1%); ASTM-D638
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature 23.0 °C
13100 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature -40.0 °C
13100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 3.0%); ASTM-D638
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature 23.0 °C
13100 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature -40.0 °C
13100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D638
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 90.0 MPa

@Temperature 80.0 °C
13100 psi

@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..