Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 910 MPa @Thickness 1.45 mm |
132000 psi @Thickness 0.0571 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Ultimate | 910 MPa @Thickness 3.20 mm, Temperature 538 °C |
132000 psi @Thickness 0.126 in, Temperature 1000 °F |
As Welded, Solution Annealed, and Aged; Base/Base Fracture |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 909 MPa @Thickness 3.20 mm |
132000 psi @Thickness 0.126 in |
10% cold reduction |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 913 MPa @Diameter 12.7 mm |
132000 psi @Diameter 0.500 in |
As Welded and Solution Annealed at 2075°F(1135°C)/30min/AC |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 910 MPa @Thickness 12.7 mm, Temperature 538 °C |
132000 psi @Thickness 0.500 in, Temperature 1000 °F |
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |