Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 92.0 MPa

@Temperature 980 °C
13300 psi

@Temperature 1800 °F
Hot-Rolled Plate, Solution-Annealed
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy
INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex..
Tensile Strength, Ultimate 92.0 MPa

@Temperature 80.0 °C
13300 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 92.0 MPa

@Temperature 23.0 °C
13300 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D638
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 92.0 MPa

@Temperature 23.0 °C
13300 psi

@Temperature 73.4 °F
ASTM D 638
Saint-Gobain Meldin® 2001 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..