Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 93.8 MPa

@Temperature 427 °C
13600 psi

@Temperature 800 °F
18-8 stainless steel butt joint.
Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy
Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly..