Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1074 MPa @Thickness 12.7 mm, Temperature 25.0 °C |
155800 psi @Thickness 0.500 in, Temperature 77.0 °F |
As Welded, Solution Annealed, and Aged; Base/Base Fracture |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |