Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.0 MPa @Temperature 80.0 °C |
1600 psi @Temperature 176 °F |
Practical Use (Water Absorption 2.4%); ASTM-D638 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |