Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1147 MPa @Temperature 25.0 °C |
166400 psi @Temperature 77.0 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |