Tensile Strength, Ultimate 1150 MPa

@Temperature 23.0 °C
167000 psi

@Temperature 73.4 °F
Special Metals NIMONIC® Alloy 105
A precipitation-hardenable nickel-cobalt-chromium alloy with an addition of molybdenum for solid-solution strengthening. The relatively high aluminum content enhances both strength (through greater..
Tensile Strength, Ultimate 1150 MPa

@Temperature 23.0 °C
167000 psi

@Temperature 73.4 °F
Special Metals NIMONIC® Alloy 90
A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to..
Tensile Strength, Ultimate 1150 MPa

@Temperature 23.0 °C
167000 psi

@Temperature 73.4 °F
Special Metals NIMONIC® Alloy PK33
A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h..