Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1520 MPa

@Temperature 204 °C
220000 psi

@Temperature 400 °F
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..
Tensile Strength, Ultimate 1520 MPa

@Temperature 316 °C
220000 psi

@Temperature 600 °F
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..