Polymer Property : Tensile Strength, Ultimate = 241 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 241 MPa

@Temperature 288 °C
34900 psi

@Temperature 550 °F
Transverse
ATI Wah Chang Zirconium Alloy Zircaloy-4
Zirconium resists corrosive attack in most organic and mineral acids, strong alkalis, and some molten salts. A tightly adherent and protective oxide film protects the metal-oxide interface to provid..