Polymer Property : Tensile Strength, Ultimate = 2450 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2450 MPa

@Temperature 371 °C
355000 psi

@Temperature 700 °F
AGY ADVANTEX® Generic Glass Fiber
OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.Information provided by AGY Holding Corp...