Polymer Property : Tensile Strength, Ultimate = 338 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 338 MPa

@Temperature 260 °C
49000 psi

@Temperature 500 °F
Stainless Steel (18-8) butt joint
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet..