Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 395 MPa @Thickness 1.60 mm |
57300 psi @Thickness 0.0630 in |
L Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |