Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 441 MPa

@Thickness 3.17 mm
>= 64000 psi

@Thickness 0.125 in
45° Direction
Alcoa 2090-T83 Aluminum
Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has ..
Tensile Strength, Ultimate 441 MPa

@Diameter 12.7 mm,
Temperature 538 °C
64000 psi

@Diameter 0.500 in,
Temperature 1000 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..