Polymer Property : Tensile Strength, Ultimate = 500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 500 MPa

@Temperature 425 °C
72500 psi

@Temperature 797 °F
Solution Annealed prior to test
Special Metals INCOLOY® Alloy DS
A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista..
Tensile Strength, Ultimate 500 MPa

@Temperature 550 °C
72500 psi

@Temperature 1020 °F
Solution Annealed prior to test
Special Metals INCONEL® Alloy G-3
A nickel-chromium-iron alloy with additions of molybdenum and copper. It has good weldability and resistance to intergranular corrosion in the welded condition. The low carbon content helps preven..
Tensile Strength, Ultimate 500 MPa

@Thickness >=508 mm
72500 psi

@Thickness >=20.0 in
at center (L/T direction)
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..